ABSTRACT:
A method for strengthening and increasing the thickness of the strengthened surface layer of a dental ceramic restorative material where the ceramic material is heat treated with a salt composition containing a lithium ion and a metal ion larger than the lithium ion first at a temperature above the strain temperature followed by a second heat treatment with the salt composition at a temperature below the strain temperature. The treatment is especially effective for all-ceramic, high-leucite feldspathic porcelain restorations.
REFERENCES:
patent: 2779136 (1957-01-01), Hood et al.
patent: 3395998 (1968-08-01), Olcott
patent: 3630704 (1971-12-01), Garfinkel et al.
patent: 3751238 (1973-08-01), Grego et al.
patent: 3765855 (1973-10-01), Larrick
patent: 3798013 (1974-03-01), Inoue et al.
patent: 3853674 (1974-12-01), Levene
patent: 3879274 (1975-04-01), Matsumori et al.
patent: 4206253 (1980-06-01), Watanabe
patent: 4483700 (1984-11-01), Forker, Jr. et al.
patent: 4546006 (1985-10-01), Ohno et al.
patent: 4550030 (1985-10-01), Ohi et al.
patent: 4702760 (1987-10-01), Garcia de Leon
patent: 4784606 (1988-11-01), Jones et al.
patent: 4798536 (1989-01-01), Katz
patent: 4872896 (1989-10-01), LaCourse et al.
patent: 5071801 (1991-12-01), Bedard et al.
patent: 5077132 (1991-12-01), Maruno et al.
patent: 5453290 (1995-09-01), van der Zel
Crimaldi, A.J. et al., "Strengthening of Leucite-reinforced Porcelain by Double Ion Exchange." General Session and Exhibition of the International Association for Dental Research, Poster Session, Thursday, Mar. 10, 1994.
Denry, I.L. et al., "Enhanced Chemical Strengthening of Feldspathic Dental Porcelain." Journal of Dental Research, vol.72, No. 10(Oct. 1993), pp. 1429-1433.
Dunn, B. et al., "Improving the Fracture Resistance of Dental Ceramic." Journal of Dental Research, vol. 56, No. 10,(Oct. 1977), pp. 1209-1213.
Nordberg, M.E., et al., "Strengthening by Ion Exchange." Journal of the American Ceramic Society, vol. 47, No. 5(1964), pp. 215-219, (no month).
Vaidyanathan, T.K., et al., "Properties of a New Dental Porcelain." Scanning Microscopy, vol. 3, No. 4(1989), pp. 1023-1033, (no month).
Varshneya, Arun K. et al., "Technology of Ion Exchange Strengthening of Glass: A Review." in Varshneya A.K., et al Fusion and Processing of Glass (Westerville, Ohio, American Ceramic Society, 1993), pp. 365-376, (no month).
Denry Isabelle L.
Rosenstiel Stephen F.
Dudash Diana
Pollick Philip J.
The Ohio State University
LandOfFree
Method for strengthening dental restorative materials does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for strengthening dental restorative materials, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for strengthening dental restorative materials will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2327576