ABSTRACT:
A process for reducing the average particle size of an ammonium paratungstate powder having the steps of heating the ammonium paratungstate powder at a temperature of between about 110.degree. C. to about 205.degree. C. for a time sufficient to reduce the average particle size of the ammonium paratungstate powder by at least 20 percent.

REFERENCES:
patent: 3175881 (1965-03-01), Chiola et al.
patent: 4504461 (1985-03-01), Carpenter et al.
patent: 4557923 (1985-12-01), Powers et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for reducing the average particle size of ammonium parat does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for reducing the average particle size of ammonium parat, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for reducing the average particle size of ammonium parat will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1971035

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.