Synthetic resins or natural rubbers -- part of the class 520 ser – Synthetic resins – Mixing of two or more solid polymers; mixing of solid...
Patent
1992-05-08
1993-06-08
Ziegler, Jacob
Synthetic resins or natural rubbers -- part of the class 520 ser
Synthetic resins
Mixing of two or more solid polymers; mixing of solid...
525271, 525299, 525301, 525309, 5253303, C08F26704
Patent
active
052180530
ABSTRACT:
Polymers comprising anionically polymerized monomers such as butadiene or styrene and adjacent units of (1-methyl-1-alkyl)alkyl esters such as t-butylmethacrylate, as well as selectively hydrogenated derivatives thereof, are heated to at least 180.degree. C. to convert the adjacent ester units to stable anhydride rings.
REFERENCES:
patent: 3948846 (1976-04-01), Waters
patent: 5098959 (1992-03-01), McGrath et al.
Shell Oil Company
Ziegler Jacob
LandOfFree
Polymers having stable anhydride rings does not yet have a rating. At this time, there are no reviews or comments for this patent.