ABSTRACT:
Alumina having a surface area from about 250 to about 500 m.sup.2 /g, a loose bulk density from about 10 to about 30 lbs/ft.sup.3, a pore volume (0-10,000 A) from about 0.6 to about 2.5 cc/g and a pore volume (0-1,000 A) of at least 0.6 cc/g wherein 70 to 95 percent of said pore volume (0-1,000 A) consists of pores having a diameter in the range of 35 to 80 A and a method for producing such alumina by the water hydrolysis of aluminum methoxide.

REFERENCES:
patent: 2805920 (1957-09-01), Richardson
patent: 3055737 (1962-09-01), Wilson et al.
patent: 3264061 (1966-08-01), Kehl
patent: 3264063 (1966-08-01), Carter
patent: 3352636 (1967-11-01), Wilson et al.
patent: 3394990 (1968-07-01), Weingaertner et al.
patent: 3417030 (1968-12-01), O'Hara
patent: 3419352 (1968-12-01), Acciarri
patent: 3520654 (1970-07-01), Carr et al.
patent: 3647374 (1972-03-01), Nomura et al.
patent: 3773691 (1973-11-01), Leach

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Producing alumina having a majority of pore diameters of 35-80A does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Producing alumina having a majority of pore diameters of 35-80A, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Producing alumina having a majority of pore diameters of 35-80A will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1834858

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.