ABSTRACT:
The production of grain oriented silicon steel sheets comprises a combination of hot rolling step, cold rolling step, decarburization and primary recrystallization annealing step, annealing separator applying step and secondary recrystallization annealing and purification annealing step. In this case, the cold rolled sheet is subjected to an electrolytic degreasing in a silicate bath containing an iron concentration of 50-5000 mg/l, and Cu is adhered to the surface(s) of the sheet after the decarburization and primary recrystallization annealing in an amount of 400-2000 mg/m.sup.2 per one-side surface.

REFERENCES:
patent: 4178194 (1979-12-01), Atterri et al.
patent: 4642141 (1987-02-01), Iida et al.
patent: 4975127 (1990-12-01), Kurosawa et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of producing grain oriented silicon steel sheets having i does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of producing grain oriented silicon steel sheets having i, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of producing grain oriented silicon steel sheets having i will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1827206

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.