ABSTRACT:
Hardened machined parts are manufactured from rolled or forged steel which consists essentially of 0.05 to 0.15 wt % of C, up to 0.50 wt % of Si, up to 1.5 wt % of Mn, 0.30 to 1.0 wt % of Cr, 0.50 to 1.0 wt % of Mo, one or more of elements selected from the group consisting of 0.10 to 0.40 wt % of V, 0.03 to 0.20 wt % of Ti, 0.03 to 0.20 wt % of Nb and 0.0005 to 0.0050 wt % of B, the balance being Fe, in the following steps: cooling the steel in air from 900.degree. C to 1,000.degree. C; machining the cooled steel; and subjecting the machined steel to a nitriding treatment at 500.degree. to 650.degree. C for 2 to 8 hours.

REFERENCES:
patent: 1723015 (1929-08-01), DeFries
patent: 2083208 (1937-06-01), Tofaute
patent: 2188137 (1940-01-01), Malcolm
patent: 2946708 (1960-07-01), Berghaus et al.
patent: 3901740 (1975-08-01), Anderson
Molybdenum, Steels Irons Alloys, Archer 1948, Climax Molybdenum Co., N.Y. pp. 93-96.
Metals Handbook, 8th Ed., vol. 2, 1964, pp. 119-125.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for manufacturing hardened machined parts does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for manufacturing hardened machined parts, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for manufacturing hardened machined parts will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1765155

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.