Synthetic resins or natural rubbers -- part of the class 520 ser – Synthetic resins – From silicon reactant having at least one...
Patent
1985-11-29
1986-12-23
Welsh, Maurice J.
Synthetic resins or natural rubbers -- part of the class 520 ser
Synthetic resins
From silicon reactant having at least one...
528 61, 528 65, 528 76, 528 77, 528 81, 528 83, C08G 1838
Patent
active
046313290
ABSTRACT:
The reduction in tensile strength exhibited in high humidity environments by "soft" polyurethanes prepared from aliphatic or cycloaliphatic diisocyanates can be substantially reduced if the molar ratio of diisocyanate and chain extender to isocyanate-reactive species other than said chain extender in the reaction mixtures from which said polyurethanes are prepared is at least 4.
REFERENCES:
patent: 3886226 (1975-05-01), Asai et al.
patent: 3923747 (1975-12-01), Kolycheck
patent: 4098742 (1978-07-01), Mueller
Gornowicz Gerald A.
Lee Chi-Long
Dow Corning Corporation
Spector Robert
Welsh Maurice J.
LandOfFree
Moisture resistant polyurethanes derived from non-aromatic diiso does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Moisture resistant polyurethanes derived from non-aromatic diiso, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Moisture resistant polyurethanes derived from non-aromatic diiso will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-172323