Multiphase thermoelectric alloys and method of making same

Metal treatment – Stock

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

148 115R, 148 131, 420579, 420580, 252 623T, C22C 2800

Patent

active

044472773

ABSTRACT:
There is disclosed new and improved multiphase thermoelectric alloys and a method for making the same. The alloys are disordered materials having a multiplicity of matrix crystallites separated by generally disordered grain boundaries containing transitional phases and grain boundary regions of various phases including electrically conductive phases having at least one phase having high electrical conductivity.
The alloys are formed from a mixture of at least two separately prepared multiple element compounds preferably a first compound Bi.sub.10 Sb.sub.30 Te.sub.60 or Bi.sub.40 Te.sub.48 Se.sub.12 and a second compound Ag.sub.25 Sb.sub.25 Te.sub.50. These compounds while crystalline, have different crystalline structures. They themselves are polycrystalline and do not represent the most stable crystalline structure. The first compound has a rhombohedral crystalline structure and the second compound has a face centered cubic crystalline structure. The compounds are combined in solid particulate form in proportions of 97 to 99.25 percent Bi.sub.10 Sb.sub.30 Te.sub.60 and 3 to 0.25 percent Ag.sub.25 Sb.sub.25 Te.sub.50 or 99 percent Bi.sub.40 Te.sub.48 Se.sub.12 to 1 percent Ag.sub.25 Sb.sub.25 Te.sub.50. The mixture is then heated in a quartz tube to an elevated temperature and then drawn through a temperature gradient for cooling.
The alloys include in the grain boundary regions various phases of silver and tellurium. The silver containing phases establish low resistance current paths through the crystallites to provide the alloy with high electrical conductivity. The disorder of the grain boundaries and the non-highly electrical conductive phases of the grain boundary regions provide low thermal conductivity desired for thermoelectric applications.
Also disclosed are alloys doped with a dopant such as tellurium iodide to form thermoelectric alloys having maximized S.sup.2 .sigma. products.

REFERENCES:
patent: 2957937 (1960-10-01), Jensen et al.
patent: 2995613 (1961-08-01), Wernick
patent: 3020326 (1962-02-01), Fredrick
patent: 3228805 (1966-01-01), Waseleski et al.
patent: 3256699 (1966-06-01), Henderson
patent: 3310493 (1967-03-01), Rupprecht
patent: 3414405 (1968-12-01), Fisher
RCA Abstract Quarterly Report No. 6, May 1, 1960--Jul. 31, 1960, p. IV.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Multiphase thermoelectric alloys and method of making same does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Multiphase thermoelectric alloys and method of making same, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Multiphase thermoelectric alloys and method of making same will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1601108

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.