ABSTRACT:
The stack gas from a shaft furnace in which iron ore is directly reduced is cooled and filtered and then subjected to steam so as to convert its carbon monoxide into carbon dioxide and water. The carbon dioxide and water are then scrubbed out of this stack gas so as to leave virtually pure hydrogen which is heated to a temperature between 400.degree. and 600.degree. C and added to the output of an oxygen reactor that transforms a carbon-containing substance, e.g. a hydrocarbon such as fuel oil and oxygen into a synthetic gas having a carbon-monoxide/hydrogen volume ratio of at least 0.5:1. The addition of this hydrogen to the output of the reactor lowers the volume ratio to 1:1 at most so that this mixture can be reintroduced into the shaft furnace at a temperature of around 1000.degree. C as a reducing gas.

REFERENCES:
patent: 4046555 (1977-09-01), Lange

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of the direct reduction of iron ore does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of the direct reduction of iron ore, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of the direct reduction of iron ore will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1555216

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.