ABSTRACT:
Improved toughness of forging is obtained without quenching and tempering by controlling the steel composition to: 0.05% to less than 0.15% C.; 0.10-1.00% Si; 0.50-3.00% Mn; 1.60-4.20% Mn+Cr; 0.010-0.030% Ti; 0.005-0.0030% B; 0.01-0.05% Al; and 0.0060% or less of N.
REFERENCES:
patent: 4388122 (1983-06-01), Sudo et al.
patent: 4472208 (1984-09-01), Kunishige
patent: 4537644 (1985-08-01), Tominaga et al.
Koyasu Yoshiro
Suzuki Nobukazu
Tsuchida Yutaka
Nippon Steel Corporation
Yee Deborah
LandOfFree
Non-heat refined steel bar having improved toughness does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Non-heat refined steel bar having improved toughness, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Non-heat refined steel bar having improved toughness will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1519792