Method for increasing the endurance and reducing the friction of

Coating processes – With post-treatment of coating or coating material – Heating or drying

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

252 12, 252 27, 252 29, 4273882, 4273883, B05D 302, C10M 502, C10M 704, C10M 716

Patent

active

045116067

ABSTRACT:
The present invention describes a method for increasing the endurance of oil lubricated conical roller bearings, in which the guide surface is coated with a lubricating paint that is insoluble in oil. A coating of a molybdenum disulphide lubricating paint with a thickness of 3 to 8 .mu.m is preferred. The coated bearing also exhibits reduced friction and quieter running, even when the lubricating paint has been worn off.

REFERENCES:
patent: 3717576 (1973-02-01), Hiratsuka et al.
patent: 3850820 (1974-11-01), Korshak et al.
patent: 4055503 (1977-10-01), Anselment et al.
patent: 4329238 (1982-05-01), Mitrofanova et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for increasing the endurance and reducing the friction of does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for increasing the endurance and reducing the friction of, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for increasing the endurance and reducing the friction of will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1456102

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.