ABSTRACT:
A process for making polyetherester resins is disclosed. A glycol ester of an aromatic diacid such as terephthalic acid is reacted with a polyether and a source of a dicarboxylic acid such as maleic anhydride to produce a polyetherester resin, wherein the aromatic diester content may be conveniently adjusted as desired. The process permits the preparation of unsaturated polyetherester resins with relatively high levels of terephthalate repeating units while avoiding the difficulties associated with the direct use of terephthalic acid in previously known procedures. Such unsaturated polyetheresters are useful for making thermoset resins with excellent mechanical and physical properties.
REFERENCES:
patent: 5254723 (1993-10-01), Yang et al.
patent: 5319006 (1994-06-01), Yang et al.
patent: 5436313 (1995-07-01), Klang et al.
patent: 5436314 (1995-07-01), Yang et al.
patent: 5612444 (1997-03-01), Cai et al.
Acquah Samuel A.
Arco Chemical Technology L.P.
Harper Stephen D.
LandOfFree
Process for making polyetherester resins having high aromatic di does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for making polyetherester resins having high aromatic di, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for making polyetherester resins having high aromatic di will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1425685