Ceramic cutting tool material with improved toughness

Compositions: ceramic – Ceramic compositions – Carbide or oxycarbide containing

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

501 92, 501127, 51309, C04B 3556

Patent

active

051107708

ABSTRACT:
This invention relates to a cutting tool material with improved toughness behavior using alumina or silicon nitride as the matrix material. The improved toughness is achieved by the addition of whiskers and optionally zirconia in a monoclinic or tetragonal phase, to the matrix. The whiskers are disc-shaped with a thickness of 0.5-8 .mu.m and an equivalent diameter (hypothetical diameter of a circle with the same area as the disc) of about 5-50 .mu.m.

REFERENCES:
patent: 4218253 (1980-08-01), Dworak et al.
patent: 4543345 (1985-09-01), Wei
patent: 4657877 (1987-04-01), Becher et al.
patent: 4745091 (1988-05-01), Landingham
patent: 4789277 (1988-12-01), Rhodes et al.
patent: 4804645 (1989-02-01), Ekstrom
patent: 4849381 (1989-07-01), Brandt et al.
patent: 4920838 (1990-05-01), Brandt et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Ceramic cutting tool material with improved toughness does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Ceramic cutting tool material with improved toughness, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Ceramic cutting tool material with improved toughness will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1412388

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.