ABSTRACT:
A method for making a corrosion resistant, ferritic steel alloy, with reduced magnetic coercivity is disclosed. The process includes the step of providing an intermediate form of a ferritic alloy consisting essentially of, in weight percent, about

REFERENCES:
patent: 3923560 (1975-12-01), Regitz
patent: 4244754 (1981-01-01), Masumoto et al.
patent: 4390378 (1983-06-01), Rastogi
patent: 4394192 (1983-07-01), Rastogi
patent: 4421574 (1983-12-01), Lyudkovsky
patent: 4601766 (1986-07-01), Rastogi et al.
patent: 4772341 (1988-09-01), Rastogi et al.
patent: 5091024 (1992-02-01), DeBold et al.
"Standard Specification for Low-Carbon Magnetic Iron", ASTM Designation: A 848/A848M-96 pp. 1-5 (1996).
"REMKO Soft Magnetic Iron", Technical Bulletin, Uddeholm Corporation, Totowa, NJ (1988).

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for improving magnetic performance in a free-machining f does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for improving magnetic performance in a free-machining f, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for improving magnetic performance in a free-machining f will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1391227

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.