ABSTRACT:
A high strength low density opaque shaped aluminum borate product is disclosed characterized by an MOR of at least 45,000 psi and a density of approximately 2.9 g/cm.sup.3. The shaped aluminum borate may be formed by reacting an aluminum oxide with a boron oxide at a temperature of at least 800.degree. C., grinding the reaction product, pressing the resulting particulate into a shaped form and sintering the shaped particulate at a temperature of from 800.degree. to 1400.degree. C. while maintaining the shaped particulate under a pressure of 2500 to 3500 psi.

REFERENCES:
patent: 2118143 (1938-05-01), Benner et al.
patent: 3080242 (1963-03-01), Berry
patent: 3350166 (1967-10-01), Alley et al.
patent: 3503765 (1970-03-01), Blaze
patent: 3795524 (1971-03-01), Sowman
patent: 4510253 (1985-04-01), Felice et al.
patent: 4522926 (1985-06-01), Felice et al.
patent: 4540475 (1985-09-01), DeAngelis

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Light weight shaped opaque aluminum borate product and method of does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Light weight shaped opaque aluminum borate product and method of, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Light weight shaped opaque aluminum borate product and method of will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1365597

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.