Process for producing hardened semicoke briquettes

Fuel and related compositions – Liquid fuels – Aluminum or heavy metal – other than lead – containing

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

44 10C, 201 5, C10L 516, C10L 540

Patent

active

041652207

ABSTRACT:
Briquettes obtained from semicoke and a binder such as pitch, can be hardened when stacked to relatively great height of 5 to 10 meters, provided the "green" briquettes are heated in a vertical oven at a temperature between 300.degree. C. and 400.degree. C. for 35 to 50 minutes in an inert atmosphere such as nitrogen.

REFERENCES:
patent: 3926576 (1975-12-01), Schmalfeld et al.
patent: 3969088 (1976-07-01), Mansfield et al.
patent: 4039319 (1977-08-01), Schapiro et al.
patent: 4050990 (1977-09-01), Lorenz

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for producing hardened semicoke briquettes does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for producing hardened semicoke briquettes, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for producing hardened semicoke briquettes will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1322127

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.