ABSTRACT:
Composite metal/porcelain tooth reconstructions are manufactured by bonding porcelain to a basis metal which is pretreated by electrolytically depositing thereon a thin layer of a different metal. The pretreatment has the effect of increasing the bond strength between the metal and the porcelain.
If the basis metal is a noble metal, the different metal may be deposited directly, and the porcelain then bonded on. If the basis metal is a base metal the pretreatment preferably includes an etching step, deposition of a preliminary metal layer on the etched surface, followed by deposition of the main metal layer, followed by a final deposition of metal prior to bonding to the porcelain.
REFERENCES:
patent: 1782552 (1930-11-01), Supplee
patent: 2569453 (1951-10-01), Chester et al.
patent: 2819207 (1958-01-01), Shepard
patent: 2980998 (1961-04-01), Coleman et al.
patent: 3585064 (1971-06-01), Prosen
Modern Electroplating; Frederick A. Lowenheim, editor; John Wiley & Sons, Inc; New York, 1963, p. 434.
Leader William
Mack John H.
LandOfFree
Artificial teeth construction does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Artificial teeth construction, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Artificial teeth construction will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1300330