Method of producing flint

Metal treatment – Compositions – Heat treating

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

75152, 148 3, B22D 2500, C22C 2300

Patent

active

040897060

ABSTRACT:
Flint is produced from a mischmetal and iron melt by permitting the alloy melt to cool in a mold at a slow enough rate that, as the solidification point of the melt is approached, its temperature is maintained at 800.degree.-600.degree. C for at least 10 minutes. The alloy melt is subsequently extruded and the extrudate is subjected to a heat treatment at temperatures from 370.degree.-470.degree. C for 1/2 to 4 hours, the heat treatment being discontinued before the limit value of the thermodynamic equilibrium has been reached.

REFERENCES:
patent: 2792301 (1957-05-01), Bungardt
patent: 3236633 (1966-02-01), Bungardt
patent: 3839101 (1974-10-01), Doser
patent: 3839102 (1974-10-01), Tawara et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of producing flint does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of producing flint, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of producing flint will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1196019

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.