ABSTRACT:
Processing of pearlite by treating the same with an alkaline solution having a concentration of 40-140 g/l taken in an amount which brings the ratio of the liquid and solid phases to (0.7-1.5) : 1 and then separating by filtration the water glass, obtained in the process of heat treatment, from the residue formed.

REFERENCES:
patent: 1945534 (1934-02-01), Rembert
patent: 2047614 (1936-07-01), Cavezzale
patent: 2078836 (1937-04-01), Carter
patent: 3101251 (1963-08-01), Howell
patent: 3515682 (1970-06-01), Flank et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Processing pearlite to obtain metal silicates does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Processing pearlite to obtain metal silicates, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Processing pearlite to obtain metal silicates will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-10552

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.