ABSTRACT:
A wrought Al/Cu/Mg type aluminum alloy of high strength in the temperature range between 0 and 250.degree. C., having the following composition:

REFERENCES:
patent: 3288601 (1966-11-01), Flemings et al.
patent: 3475166 (1969-10-01), Raffin
patent: 3925067 (1975-12-01), Sperry et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Wrought Al/Cu/Mg-type aluminum alloy of high strength in the tem does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Wrought Al/Cu/Mg-type aluminum alloy of high strength in the tem, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Wrought Al/Cu/Mg-type aluminum alloy of high strength in the tem will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1746667

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.