ABSTRACT:
A wet-stick pressure-sensitive adhesive is provided wherein the pressure-sensitive adhesive comprises: at least one copolymerized monoethylenically unsaturated (meth)acrylic acid ester monomer, wherein the (meth)acrylic acid ester monomer, when homopolymerized, has a Tg of less than about 10° C.; at least one copolymerized hydrophilic acidic comonomer; and at least one nonreactive copolymer comprising at least two copolymerized alkylene oxides, at least one of which is hydrophobic and at least one of which is hydrophilic.

REFERENCES:
patent: RE24906 (1960-12-01), Ulrich
patent: 3234062 (1966-02-01), Morris
patent: 3449184 (1969-06-01), Balk
patent: 3681179 (1972-08-01), Theissen
patent: 3772262 (1973-11-01), Clementi
patent: 3786116 (1974-01-01), Milkovich et al.
patent: 3842059 (1974-10-01), Milkovich et al.
patent: 3867222 (1975-02-01), Plant et al.
patent: 4035549 (1977-07-01), Kennar
patent: 4181752 (1980-01-01), Martens et al.
patent: 4188436 (1980-02-01), Ellis et al.
patent: 4234533 (1980-11-01), Langlands
patent: 4299639 (1981-11-01), Bayer
patent: 4303485 (1981-12-01), Levens
patent: 4329384 (1982-05-01), Vesley
patent: 4330590 (1982-05-01), Vesley
patent: 4341576 (1982-07-01), Lewis
patent: 4358329 (1982-11-01), Masuda
patent: 4359547 (1982-11-01), Agarwal et al.
patent: 4362587 (1982-12-01), Baudin et al.
patent: 4379201 (1983-04-01), Heilmann
patent: 4385951 (1983-05-01), Pressau
patent: 4386991 (1983-06-01), Shiomi et al.
patent: 4431471 (1984-02-01), Mertens et al.
patent: 4452840 (1984-06-01), Sato et al.
patent: 4465729 (1984-08-01), Cancio et al.
patent: 4543283 (1985-09-01), Curtze et al.
patent: 4554324 (1985-11-01), Husman
patent: 4569960 (1986-02-01), Blake
patent: 4595001 (1986-06-01), Potter et al.
patent: 4598004 (1986-07-01), Heinecke
patent: 4599274 (1986-07-01), Ando et al.
patent: 4619979 (1986-10-01), Kotnour et al.
patent: 4671913 (1987-06-01), Gen et al.
patent: 4737559 (1988-04-01), Kellen
patent: 4843134 (1989-06-01), Kotnour et al.
patent: 4871812 (1989-10-01), Lucast et al.
patent: 4925725 (1990-05-01), Endo et al.
patent: 4952618 (1990-08-01), Olsen
patent: 5049608 (1991-09-01), Medina
patent: 5091258 (1992-02-01), Moran
patent: 5100963 (1992-03-01), Lin
patent: 5125995 (1992-06-01), D'Haese et al.
patent: 5147485 (1992-09-01), Gajewski et al.
patent: 5178933 (1993-01-01), Yoshida et al.
patent: 5180756 (1993-01-01), Rehmer et al.
patent: 5190992 (1993-03-01), Kato et al.
patent: 5254388 (1993-10-01), Melby et al.
patent: 5268049 (1993-12-01), Marriott et al.
patent: 5362801 (1994-11-01), Amici et al.
patent: 5397614 (1995-03-01), Patnode et al.
patent: 5407971 (1995-04-01), Everaerts et al.
patent: 5425977 (1995-06-01), Hopfe
patent: 5429590 (1995-07-01), Saito et al.
patent: 5436283 (1995-07-01), Okada et al.
patent: 5441998 (1995-08-01), Teeters et al.
patent: 5445890 (1995-08-01), Bayha et al.
patent: 5455103 (1995-10-01), Hoagland et al.
patent: 5461103 (1995-10-01), Bafford et al.
patent: 5487412 (1996-01-01), Matthews et al.
patent: 5506279 (1996-04-01), Babu
patent: 5536347 (1996-07-01), Moran
patent: 5547736 (1996-08-01), Simon et al.
patent: 5595818 (1997-01-01), Hopfe et al.
patent: 5613942 (1997-03-01), Lucast et al.
patent: 5620779 (1997-04-01), Levy et al.
patent: 5637646 (1997-06-01), Ellis
patent: 5716701 (1998-02-01), Skoglund et al.
patent: 5733570 (1998-03-01), Chen et al.
patent: 5741542 (1998-04-01), Williams et al.
patent: 5750134 (1998-05-01), Scholz et al.
patent: 5753768 (1998-05-01), Ellis
patent: 5785985 (1998-07-01), Czech et al.
patent: 5804610 (1998-09-01), Hamer et al.
patent: 5876855 (1999-03-01), Wong et al.
patent: 5939479 (1999-08-01), Reaves et al.
patent: 5969069 (1999-10-01), Su
patent: 5976690 (1999-11-01), Williams et al.
patent: 3926897 (1991-03-01), None
patent: 4406978 (1994-03-01), None
patent: 19522792 (1995-06-01), None
patent: 4432368 (1996-03-01), None
patent: 196 28 999 (1998-03-01), None
patent: 0 099 087 (1984-01-01), None
patent: 0 056 719 (1987-05-01), None
patent: 91800 (1992-09-01), None
patent: 0 525 403 (1993-02-01), None
patent: 353972 (1994-01-01), None
patent: 0 593 231 (1994-02-01), None
patent: 0 593 231 (1994-04-01), None
patent: 670338 (1995-09-01), None
patent: 0 670 338 (1995-09-01), None
patent: 0 701 822 (1996-03-01), None
patent: 0 710 545 (1996-05-01), None
patent: 853 092 (1998-07-01), None
patent: 2 155 856 (1985-10-01), None
patent: 51-89540 (1976-08-01), None
patent: 8295850 (1995-04-01), None
patent: 96073826 (1996-03-01), None
patent: WO92/04418 (1992-03-01), None
patent: WO93/10177 (1993-05-01), None
patent: WO 93/10177 (1993-05-01), None
patent: WO95/27014 (1995-10-01), None
patent: WO 95/27014 (1995-10-01), None
patent: WO97/07161 (1997-02-01), None
patent: WO98/03208 (1998-01-01), None
patent: WO98/29516 (1998-07-01), None
patent: WO99/14415 (1999-03-01), None
J. Yamashita, et al.,Polymer Journal, 14, 255-260 (1982).
K. Ito et al.,Macromolecules, 13, 216-221 (1980).
Textbook of Polymer Science, Second. Ed., publ. Wiley-Interscience, pp. 84-85 (1971).
Masters, K.,Spray Drying: An Introduction to Principles, Operational Practice, and Application, 2nd Edition, Wiley, NY 1976, pp. 74-93.
Satas, D.,The Handbook of Pressure Sensitive Adhesive Technology, 2nd Edition, Van Nostrand Reinhold, NY, 1989, pp. 172-173.
ASTM Designation: D 3654M-88 (Reapproved 1993), Standard Test Method for Holding Power of Pressure-Sensitive Tapes (Metric).
Fox, T. G., Bulletin of the American Physical Society (ser. 2), 12.3, J5 (1956).
Kirk-Othmer Encyclopedia of Chemical Technology, 4th Edition, John Wiley & Sons, NY, vol. 6, 1993, pp. 635-636.
Nichols, R. T. and R. M. Sowers, “Laminated Materials, Glass,”Kirk-Othmer Encyclopedia of Chemical Technology, 4th Ed., pp. 1059-1074, 1995.
Sung Gun Chu, Chapter 8, Handbook of Pressure Sensitive Adhesive Technology, Second Edition, Donatas Satas, Editor, pp. 158-203, 1989.
Patent Abstracts of Japan, vol. 1995, No. 1, Feb. 28, 1995 & JP 06285978, Oct. 11, 1994 (abstract).
“BASF Performance Chemicals Pluronic® and Tetronic® Surfactants,” BASF Product Information Brochure, Title page, Table of Contents, and pp. 1-5 (1996).

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Wet-stick adhesives, articles, and methods does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Wet-stick adhesives, articles, and methods, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Wet-stick adhesives, articles, and methods will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3512491

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.