ABSTRACT:
A method of repairing a void on a nickel or cobalt base superalloy investment casting by vibrating the casting for a time before repairing the void, vibrating the casting while filling the void wherein the void is filled by repeatedly making incremental weld deposits of a superalloy filler material in the void using pulsed gas tungsten arc welding, and impinging each incremental deposit with a cooling gas after each incremental weld deposit is made and before the next incremental weld deposit is made, and vibrating the casting for a time after the void is filled.

REFERENCES:
patent: 1939712 (1933-12-01), Mahoux
patent: 2848775 (1958-08-01), Ettenreich
patent: 2908801 (1959-10-01), Cresswell
patent: 3274033 (1966-09-01), Jacke
patent: 3622404 (1971-11-01), Thompson
patent: 3677831 (1972-07-01), Pezaris et al.
patent: 3741820 (1973-06-01), Hebel, Jr. et al.
patent: 3864542 (1975-02-01), Fletcher et al.
patent: 4381673 (1983-05-01), Klauba et al.
patent: 4386727 (1983-06-01), Unde
patent: 4409462 (1983-10-01), Jahnke
patent: 4711986 (1987-12-01), Lillquist et al.
patent: 4823599 (1989-04-01), Schneider
patent: 4878953 (1989-11-01), Saltzman et al.
patent: 4968359 (1990-11-01), Hebel, Jr. et al.
patent: 5086207 (1992-02-01), Deam
patent: 5831241 (1998-11-01), Amos
patent: 6120624 (2000-09-01), Vogt et al.
patent: 6223974 (2001-05-01), Unde
patent: 39 42 079 (1991-06-01), None
patent: 0 491 189 (1992-06-01), None
patent: 53022841 (1978-03-01), None
patent: 61193776 (1986-08-01), None

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Weld repair of superalloy castings does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Weld repair of superalloy castings, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Weld repair of superalloy castings will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3372295

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.