ABSTRACT:
Aluminum-lithium plates are butt-welded by juxtaposing the plates and making a preliminary weld from the rear or root side of the seam. An initial weld is then made from the face side of the seam, which may cause a defect in the root portion. A full-size X-ray is made and overlain over the seam to identify the defects. The defect is removed from the root side, and rewelded. Material is then removed from the face side, and the cavity is rewelded. The procedure repeats, alternating from the root side to the face side, until the weld is sound.

REFERENCES:
patent: 3192618 (1965-07-01), Altgelt
patent: 4049186 (1977-09-01), Hanneman et al.
patent: 4285459 (1981-08-01), Baladjanian et al.
patent: 4458125 (1984-07-01), Leis
patent: 4493451 (1985-01-01), Clark et al.
patent: 4575611 (1986-03-01), Bertossa
patent: 4624402 (1986-11-01), Pitcairn et al.
patent: 4959523 (1990-09-01), Fihey et al.
patent: 5071054 (1991-12-01), Dzugan et al.
patent: 5156321 (1992-10-01), Liburdi et al.
patent: 5258600 (1993-11-01), Arthur

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Weld repair method for aluminum lithium seam does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Weld repair method for aluminum lithium seam, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Weld repair method for aluminum lithium seam will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1624191

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.