ABSTRACT:
A wear-resistant alloy comprising boron, chromium and iron having maximum hardness for a given composition is produced by rapidly cooling and solidfying spheroidal particles of the molten alloy mixture. The resultant solid particles are then cast in the desired form, or incorporated into a composite alloy wherein the solid particles are held together with a matrix of different material from the alloy.

REFERENCES:
patent: 2567121 (1951-09-01), Olsen

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Wear-resistant alloy, and method of making same does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Wear-resistant alloy, and method of making same, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Wear-resistant alloy, and method of making same will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-554527

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.