ABSTRACT:
A multilayer adhesive construction and method for production of said construction are provided. The construction comprises a facestock, a barrier layer on the facestock, and an adhesive layer on the barrier layer. The barrier layer comprises a pressure-sensitive adhesive which inhibits the migration of mobile species such as oils, resins, tackifiers, or plasticizers from the adhesive layer into the facestock or from the facestock into the adhesive layer. This migration of mobile ingredients often manifests itself as swelling or hardening of the facestock which, in turn, leads to wrinkling of the adhesive construction and general loss of adhesion. The multilayer adhesive construction of the invention thus improves adhesion and the appearance of the label by inhibiting wrinkling and/or staining.
REFERENCES:
patent: 3464842 (1969-09-01), Jackstadt
patent: 3547852 (1970-12-01), Burke, Jr.
patent: 4045600 (1977-08-01), Williams
patent: 4086388 (1978-04-01), Brown
patent: 4112177 (1978-09-01), Salditt et al.
patent: 4175156 (1979-11-01), Ikins
patent: 4260659 (1981-04-01), Gobran
patent: 4284681 (1981-08-01), Tidmarsh et al.
patent: 4335171 (1982-06-01), Zenk
patent: 4374883 (1983-02-01), Winslow
patent: 4543139 (1985-09-01), Freedman et al.
patent: 4577204 (1986-03-01), Shibata et al.
patent: 4581281 (1986-04-01), Gerace
patent: 4605592 (1986-08-01), Paquette et al.
patent: 4822676 (1989-04-01), Mudge
patent: 4892917 (1990-01-01), Mudge
patent: 4894259 (1990-01-01), Kuller
patent: 4908268 (1990-03-01), Mudge
patent: 4939220 (1990-07-01), Mudge
patent: 4943461 (1990-07-01), Karin
patent: 4968558 (1990-11-01), Briddell et al.
patent: 4968559 (1990-11-01), Hideo et al.
patent: 5000810 (1991-03-01), Silverstein
patent: 5089320 (1992-02-01), Straus et al.
patent: 5189126 (1993-02-01), Bernard
patent: 5229207 (1993-07-01), Paquette et al.
patent: 5232958 (1993-08-01), Mallya et al.
patent: 5248808 (1993-09-01), Bernard et al.
patent: 5290842 (1994-03-01), Sasaki et al.
patent: 5302649 (1994-04-01), Sasaki et al.
patent: 5304418 (1994-04-01), Akada et al.
patent: 5322876 (1994-06-01), Sasaki et al.
patent: 5354600 (1994-10-01), Fisher et al.
patent: 5558913 (1996-09-01), Sasaki et al.
Chemical Abstracts, vol. 104, No. 14, p. 61, Apr. 7, 1986, Columbus, Ohio, abstract No. 111067, "Pressure Sensitive Adhesive tapes and Films".
Technical Data Sheet from Schenectady International for Acrylic Polymer HRJ-4527.
Technical Data Sheet from Schenectady International for Acrylic Polymer HRJ-10753.
Technical Data Sheet from Schenectady International for Acrylic Polymer HRJ-12531.
Ang T. Liem
Sartor Luigi
Ugolick Ronald
Avery Dennison Corporation
Zirker Daniel
LandOfFree
Use of pressure-sensitive adhesive as a barrier coating does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Use of pressure-sensitive adhesive as a barrier coating, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Use of pressure-sensitive adhesive as a barrier coating will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1669129