ABSTRACT:
The present invention is directed to a method to stabilize aluminum ions in recirculating water systems comprising adding to the system 0.1 to 1,000 ppm of a water-soluble polymer having an intrinsic viscosity of 0.05 to 2.5 dl/g in 1.0 M NaCl, prepared from:
(A) 35 to 90%, by weight, of an unsaturated carboxylic compound selected from the group consisting of acrylic acid, methacrylic acid, their salts and mixtures thereof; and
(B) 10 to 65%, by weight, of an unsaturated sulfonic compound selected from the group consisting of 2-acrylamido-2-methylpropylsulfonic acid, 2-methacrylamido-2-methylpropylsulfonic acid, their salts and mixtures thereof.

REFERENCES:
patent: 3709816 (1973-01-01), Walker et al.
patent: 3806367 (1974-04-01), Lange et al.
patent: 3928196 (1975-12-01), Persinski et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Use of carboxylic acid/sulfonic acid copolymers as aluminum ion does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Use of carboxylic acid/sulfonic acid copolymers as aluminum ion , we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Use of carboxylic acid/sulfonic acid copolymers as aluminum ion will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1383395

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.