ABSTRACT:
A stainless cast steel of ferrite-austenite two-phase structure having high corrosion fatigue strength and high pitting corrosion resistance containing in terms of % by weight, up to 0.1% C, up to 2.0% Si, up to 2.0% Mn, 22.0-27.0% Cr, 5.0-9.0% Ni, 1.1-2.5% Mo, 0.5-2.5% Cu, 0.5-2.0% Co and 0.5-2.0% V, the steel further containing, if desired, one or more kinds of 0.5-2.0% Nb and/or Ta and 0.01-0.5% Ti, the balance being substantially Fe and inevitable impurities.

REFERENCES:
patent: Re28523 (1975-08-01), Hill et al.
Reed-Hill, Robert, Physical Metallurgy Principles, 2nd Ed., 1973, p. 813.
Brick et al., Structure and Properties of Engineering Materials, 4th Ed., 1977, pp. 458-459.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Two-phase stainless cast steel having high corrosion fatigue str does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Two-phase stainless cast steel having high corrosion fatigue str, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Two-phase stainless cast steel having high corrosion fatigue str will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1022942

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.