ABSTRACT:
A process is provided for treating 7000 series aluminum alloys whereby their stress-corrosion resistance is greatly increased. In accordance with the process, the alloy is pre-aged, deformed at room temperature, and then subjected to two aging steps. The alloy so treated has a high resistance to stress corrosion while retaining satisfactory strength properties.
REFERENCES:
patent: 2083576 (1937-06-01), Nock
patent: 2506788 (1950-05-01), Hobbs
patent: 2865796 (1958-12-01), Rosenkranz
patent: 3133839 (1964-05-01), Thomas
patent: 3791880 (1974-02-01), Hunsicker et al.
patent: 3836405 (1974-09-01), Staley et al.
Lyman, T. et al.; Metals Handbook (I), Cleveland, 1961 (ASM) p. 948.
Brisbane Alton W.
Reimann Walter H.
Kuhn Cedric H.
Rusz Joseph E.
Satterfield Walter R.
The United States of America as represented by the Secretary of
LandOfFree
Treatment of aluminum alloys does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Treatment of aluminum alloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Treatment of aluminum alloys will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-519276