ABSTRACT:
Stress corrosion cracking of austenitic stainless steel or nickel-based alloys attributable at least in part to exposure to irradiation is reduced with a specific heat treatment.
REFERENCES:
patent: 2172428 (1939-09-01), Wulff et al.
patent: 2527287 (1950-10-01), Ziegler et al.
patent: 2553330 (1961-05-01), Post et al.
patent: 2553707 (1951-05-01), Goller
patent: 3253966 (1966-05-01), Malagari et al.
patent: 3340048 (1967-09-01), Floreco
patent: 3563813 (1971-02-01), Webster
patent: 3650845 (1972-03-01), Oda et al.
patent: 3756865 (1973-09-01), Sastri
patent: 3839100 (1974-10-01), Ota
patent: 4022640 (1977-05-01), Tanczya
patent: 4042421 (1977-08-01), Sype et al.
patent: 4224062 (1980-09-01), Darnfors
patent: 4227923 (1980-10-01), Watanabe et al.
Gordon Gerald M.
Jacobs Alvin J.
Dean R.
General Electric Company
Schroeder Robert R.
Simkins Raymond G.
LandOfFree
Treatment for overcoming irradiation induced stress corrosion cr does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Treatment for overcoming irradiation induced stress corrosion cr, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Treatment for overcoming irradiation induced stress corrosion cr will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-409702