Treatment for inhibiting irradiation induced stress corrosion cr

Metal treatment – Process of modifying or maintaining internal physical... – Chemical-heat removing or burning of metal

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

148135, C21B 600

Patent

active

048789623

ABSTRACT:
A heat treatment method for inhibiting irradiation induced stress corrosion cracking in stainless steel and related nickel-chromium alloys.

REFERENCES:
patent: 1807453 (1931-05-01), Tielke
patent: 2888373 (1959-05-01), Cherrie et al.
patent: 3052576 (1962-09-01), Josso
patent: 3131055 (1984-04-01), Behar
patent: 3384476 (1968-05-01), Egnell
patent: 3649251 (1972-03-01), Larson, Jr. et al.
patent: 3873378 (1975-03-01), Webster
patent: 3957545 (1976-05-01), Mimino et al.
patent: 4086107 (1978-04-01), Tanino et al.
patent: 4353755 (1982-10-01), Solomon
patent: 4576641 (1986-03-01), Bates et al.
patent: 4778651 (1988-10-01), Dubuisson et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Treatment for inhibiting irradiation induced stress corrosion cr does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Treatment for inhibiting irradiation induced stress corrosion cr, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Treatment for inhibiting irradiation induced stress corrosion cr will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-81717

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.