Transient liquid phase eutectic bonding

Metal fusion bonding – Process – Diffusion type

Reexamination Certificate

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C228S193000, C228S225000

Reexamination Certificate

active

07628309

ABSTRACT:
A method for bonding two components together including the steps of providing a first component, providing a second component, and locating a first eutectic bonding material between the first and second component. The first eutectic bonding material includes at least one of germanium, tin, or silicon. The method further includes the step of locating a second eutectic bonding material between the first and second component and adjacent to the first eutectic bonding material. The second eutectic bonding material includes gold. The method further includes the step of heating the first and second eutectic bonding materials to a temperature above a eutectic temperature of an alloy of the first and second eutectic bonding materials to allow a hypoeutectic alloy to form out of the first and second eutectic bonding materials. The method includes the further step of cooling the hypoeutectic alloy to form a solid solution alloy bonding the first and second components together.

REFERENCES:
patent: 3200490 (1965-08-01), Clymer
patent: 3396454 (1968-08-01), Schroeder et. al.
patent: 3619742 (1971-11-01), Rud, Jr.
patent: 3879746 (1975-04-01), Fournier
patent: 3935986 (1976-02-01), Lattari et al.
patent: 4215156 (1980-07-01), Dalal et al.
patent: 4233337 (1980-11-01), Friedman et al.
patent: 4330343 (1982-05-01), Christou et al.
patent: 4400869 (1983-08-01), Wilner et al.
patent: 4505027 (1985-03-01), Schwabe et al.
patent: 4545115 (1985-10-01), Bauer et al.
patent: 4637129 (1987-01-01), Derkits, Jr. et al.
patent: 4702941 (1987-10-01), Mitchell et al.
patent: 4722227 (1988-02-01), Grob et al.
patent: 4758534 (1988-07-01), Derkits, Jr. et al.
patent: 4777826 (1988-10-01), Rud, Jr. et al.
patent: 4910578 (1990-03-01), Okamoto
patent: 4912543 (1990-03-01), Neppl et al.
patent: 4939497 (1990-07-01), Nishida et al.
patent: 4960718 (1990-10-01), Aina
patent: 5038996 (1991-08-01), Wilcox et al.
patent: 5181417 (1993-01-01), Nishida et al.
patent: 5182218 (1993-01-01), Fujihira
patent: 5200349 (1993-04-01), Yokoyama
patent: 5285097 (1994-02-01), Hirai
patent: 5286671 (1994-02-01), Kurtz et al.
patent: 5346855 (1994-09-01), Byrne et al.
patent: 5369300 (1994-11-01), Heideman et al.
patent: 5374564 (1994-12-01), Bruel
patent: 5436491 (1995-07-01), Hase et al.
patent: 5457345 (1995-10-01), Cook et al.
patent: 5536967 (1996-07-01), Yokoyama
patent: 5559817 (1996-09-01), Derkits, Jr. et al.
patent: 5600071 (1997-02-01), Sooriakumar et al.
patent: 5637905 (1997-06-01), Carr et al.
patent: 5641994 (1997-06-01), Bollinger et al.
patent: 5665921 (1997-09-01), Gerst et al.
patent: 5670823 (1997-09-01), Kruger et al.
patent: 5675159 (1997-10-01), Oku et al.
patent: 5802091 (1998-09-01), Chakrabarti et al.
patent: 5882532 (1999-03-01), Field et al.
patent: 5882738 (1999-03-01), Blish, II et al.
patent: 5935430 (1999-08-01), Craig
patent: 5955771 (1999-09-01), Kurtz et al.
patent: 6027957 (2000-02-01), Merritt et al.
patent: 6050145 (2000-04-01), Olson et al.
patent: 6058782 (2000-05-01), Kurtz et al.
patent: 6122974 (2000-09-01), Sato et al.
patent: 6191007 (2001-02-01), Matsui et al.
patent: 6234378 (2001-05-01), Ford et al.
patent: 6272928 (2001-08-01), Kurtz
patent: 6320265 (2001-11-01), Chakrabarti et al.
patent: 6363792 (2002-04-01), Kurtz et al.
patent: 6447923 (2002-09-01), Yamakawa
patent: 6452427 (2002-09-01), Ko et al.
patent: 6465271 (2002-10-01), Ko et al.
patent: 6530282 (2003-03-01), Kurtz et al.
patent: 6564644 (2003-05-01), Kurtz
patent: 6566158 (2003-05-01), Eriksen et al.
patent: 6586330 (2003-07-01), Ludviksson et al.
patent: 6595066 (2003-07-01), Kurtz et al.
patent: 6608427 (2003-08-01), Akiyama et al.
patent: 6612178 (2003-09-01), Kurtz et al.
patent: 6706549 (2004-03-01), Okojie
patent: 6773951 (2004-08-01), Eriksen et al.
patent: 6845664 (2005-01-01), Okojie
patent: 6928878 (2005-08-01), Eriksen et al.
patent: 6932951 (2005-08-01), Losey et al.
patent: 6956268 (2005-10-01), Faris
patent: 7152482 (2006-12-01), Ueno et al.
patent: 7233094 (2007-06-01), Akiyama et al.
patent: 2003/0108674 (2003-06-01), Chung et al.
patent: 2003/0201530 (2003-10-01), Kurihara et al.
patent: 2004/0079163 (2004-04-01), Clerc et al.
patent: 2005/0042865 (2005-02-01), Cabral et al.
patent: 2005/0236710 (2005-10-01), Akiyama et al.
patent: 2006/0032582 (2006-02-01), Chen et al.
patent: 2006/0144154 (2006-07-01), Ueno et al.
patent: 10060439 (2002-06-01), None
patent: 0119691 (1984-09-01), None
patent: 0 552 466 (1992-12-01), None
patent: 0585084 (1994-03-01), None
patent: 1069419 (2001-01-01), None
patent: 2221570 (1990-02-01), None
patent: 03/103066 (2003-12-01), None
patent: 2004/031711 (2004-04-01), None
Neppl, F. et al., “A TaSixBarrier for Low Resistivity and High Reliability of Contacts to Shallow Diffusion Regions in Silicon,”Thin Solid Films, 120, pp. 257-266 (1984).
DeBlasi, J.M. et al., Characteristics of TaSi2/Poly-Si Films Oxidized in Steam for VLSI Applications,J. Electrochem. Soc.: Solid-State Science and Technology, pp. 2478-2482 (Dec. 1983).
Das, S.R., et al., “Thickness dependence of the properties and thermal stability of PtSi films,”Thin Solid Films, 253, pp. 467-472 (1994).
Holloway, K. et al., “Tantalum as a diffusion barrier between copper and silicon: Failure mechanism and effect of nitrogen addition,”J. Appl. Phys., 71(11), pp. 5433-5444 (Jun. 1992).
Crider, C.A. et al., “Platinum silicide formation under ultrahigh vacuum and controlled impurity ambients,”J. Appl. Phys.52 (4), pp. 2860-2868 (Apr. 1981).
Saraswat, K.C. et al., Thermal oxidation of tantalum silicide in O2and H2O,Appl. Phys. Lett., 41 (12), pp. 1127-1129 (Dec. 1982).
Lee, H.G., “Thermodynamic considerations of thermal oxidation of metal silicides,”Thin Solid Films, 216, pp. 230-234 (1992).
Berstein et al., “Applications of Solid-Liquid Interdiffusion (SLID) Bonding in Integrated-Circuit Fabrication,” Transactions of the Metallurgical Society of AIME, vol. 236, pp. 405-412 (Mar. 1966).
Newport Newsletter entitled “Solutions For Dispense, Assembly, and Soldering, The Newsletter of MRSI Group,” vol. III, No. 1 (Jan. 2000).
Klumpp et al., “Vertical System Integration by Using Inter-Chip Vias and Solid-Liquid lnterdiffusion Bonding,” Japanese Journal of Applied Physics, vol. 43, No. 7A, pp. L829-L830 (Jun. 11, 2004).
IZM Institut paper entitled “The SLID-ICV technigue introduced by FHG: Face-to-Face Solid Technology,” (date unknown) Applicants admit the status of this publication as prior art for the limited purpose of examination of this application, but otherwise reserve the right to challenge the status of this publication as prior art.
Garrou, “Future ICs Go Vertical,” Reed Electronics, (Feb. 1, 2005).
IZM Institut article entitled “Selected Results from Si-Technologie and Vertikale System lntefration: Vertical System Integration,” (Mar. 14, 2005).
Sinha, A.K. et al., “Effect of alloying behavior on the electrical characteristics of n-GaAs Schottky diodes metallized with W, Au, and Pt,”Appl. Phys. Lett., vol. 23, No. 12, pp. 666-668 (1973).
Guivarc'h, A. et al., “Growth of RhGa on GaAs (001) in a molecular beam epitaxy system,”Appl. Phys. Lett., 52 (12), pp. 948-950 (Mar. 21, 1988).
Sinha, A.K. et al., “n-GaAs Schottky Diodes Metallized with Ti and Pt/Ti,”SSE, vol. 19, No. 6-E, pp. 489-492 (1976).
Kumar, J. et al., “Reaction of Sputtered Pt Films on GaAs,”Phys. Chem. Solids, vol. 36, pp. 535-541 (1975).
Fukuda, M.,Reliability and Degradation of Semiconductor Lasers and LEDs, Chapter 6, Artech House, pp. 185-205 (1991).
Zengh, X.Y. et al., “Solid State Phase Equilibria in the Pt-Ga-As System,”Journal of Less-Common Metals, 146, pp. 233-239 (1989).
Lince, J.R. et al., “The growth of AuGa2thin films on GaAs (001) to form chemically unreactive interfaces,”J. Mater. Res, 1 (4), pp. 537-542 (Jul./Aug. 1986).
Okojie et al., “Stable Ti/TaSi2/Pt Ohmic Contacts on N-Type 6H-SiC Epilayer at 600

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Transient liquid phase eutectic bonding does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Transient liquid phase eutectic bonding, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Transient liquid phase eutectic bonding will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-4091871

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.