Stock material or miscellaneous articles – All metal or with adjacent metals – Honeycomb – or with grain orientation or elongated elements...
Reexamination Certificate
2006-10-03
2006-10-03
Thomas, Alexander S. (Department: 1772)
Stock material or miscellaneous articles
All metal or with adjacent metals
Honeycomb, or with grain orientation or elongated elements...
C428S608000, C428S058000, C428S061000, C428S077000, C428S078000, C428S189000, C244S131000, C244S133000
Reexamination Certificate
active
07115323
ABSTRACT:
Laminate structures and methods for forming same are disclosed. In one embodiment, a laminate structure includes a metal-polymer composite lamina. The metal-polymer composite lamina has a first face and a second face spaced apart, and extends to a terminal edge. The lamina includes a ply of fiber-reinforced polymer that extends between the first face and the second face and has an interior edge. The interior edge defines at least one cutout. A ply of metal foil extends between the first face and the second face substantially from the interior edge filling the at least one cutout.
REFERENCES:
patent: 2397415 (1946-03-01), Ghez et al.
patent: 5160771 (1992-11-01), Lambing et al.
patent: 5578384 (1996-11-01), Kingston
patent: 5693157 (1997-12-01), Kingston
patent: 5866272 (1999-02-01), Westre et al.
patent: 6039832 (2000-03-01), McCarville
patent: 6114050 (2000-09-01), Westre et al.
patent: 6194081 (2001-02-01), Kingston
patent: 6320118 (2001-11-01), Pridham et al.
patent: 6465110 (2002-10-01), Boss et al.
patent: WO 00/56541 (2000-09-01), None
Evans David W.
Li Edward
Piehl Marc J.
Sager Eric
Westre Willard
Black Lowe & Graham PLLC
The Boeing Company
Thomas Alexander S.
LandOfFree
Titanium foil ply replacement in layup of composite skin does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Titanium foil ply replacement in layup of composite skin, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Titanium foil ply replacement in layup of composite skin will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-3682232