Thermo-mechanical treatment of superalloys enabling simultaneously the production of a structure which is fine and homogeneous, with work hardened grains, a reduction in the stresses resulting from cooling and the absence of parasitic phase (Ni.sub.3 Nb-.delta. in the form of platelets for the Ni bases), characterized by an isothermal aging of predetermined duration after deformation in the final shaping sequence and in the finishing sequence which is followed by a limited amount of deformation and by a final heat treatment constituted solely by annealing producing precipitation of the hardening phase, this final treatment being optionally arranged to follow the finishing treatment, or in sequence, after cooling in air.
REFERENCES:
patent: 3676225 (1972-07-01), Owczarski et al.
Leonard Alain R.
Leray Jannick J. M. L.
Dean R.
Societe Nationale d'Etude et de Construction de Meteurs d'Aviati
LandOfFree
Thermomechanical treatment process for superalloys does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Thermomechanical treatment process for superalloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Thermomechanical treatment process for superalloys will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-983046