ABSTRACT:
A thermomechanical treatment for producing useful microstructures in the nickel base superalloys is described. The process is applied to material which has been placed in a condition of super-plasticity, and utilizes isothermal hot deformation under conditions which produce a uniform dislocation density and a resultant propensity for abnormal grain growth. The material is then recrystallized in a thermal gradient to produce a final structure consisting of elongated grains.

REFERENCES:
patent: 3519419 (1970-07-01), Gibson et al.
patent: 3702791 (1972-11-01), Freche et al.
patent: 3772090 (1973-11-01), Allen et al.
patent: 3825420 (1974-07-01), Ewing et al.
patent: 3850702 (1974-11-01), Buchanan
patent: 3920489 (1975-11-01), Buchanan

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Thermomechanical treatment for nickel base superalloys does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Thermomechanical treatment for nickel base superalloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Thermomechanical treatment for nickel base superalloys will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1484301

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.