ABSTRACT:
A heat treatment is described for producing a desired microstructure in Hastelloy Alloy X components which have small diameter, closely spaced, laser pierced holes therein. The heat treatment produces a small grain size and discontinuous carbide morphology in the component prior to the hole piercing operation, which reduces the propensity for cracking which has been found to be associated with the hole piercing operation. After the piercing operation, the component is heat treated again to increase the grain size and produce a microstructure which provides the optimum balance of creep strength and fatigue strength.
REFERENCES:
patent: 4490186 (1984-12-01), Sines et al.
Ault Earle A.
Field Thomas T.
Murrin Thomas A.
Dean R.
Rashid James M.
United Technologies Corporation
LandOfFree
Thermal treatment of wrought, nickel base superalloys in conjunc does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Thermal treatment of wrought, nickel base superalloys in conjunc, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Thermal treatment of wrought, nickel base superalloys in conjunc will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2423087