ABSTRACT:
Alpha olefins may be oligomerized over a boron trifluoride catalyst and a protonic promoter, and then held at a temperature between 60.degree. and 150.degree. C. to increase the molecular weight of the oligomers. When the oligomers are hydrogenated they provide a synthetic lubricant base stock having excellent properties. The alpha olefins may be derived from ethylene polymerization or wax pyrolysis. An inert organic solvent may be present.

REFERENCES:
patent: 4172855 (1979-10-01), Shubkin et al.
patent: 4225739 (1980-09-01), Nipe et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Thermal treatment of olefin oligomers via a boron trifluoride pr does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Thermal treatment of olefin oligomers via a boron trifluoride pr, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Thermal treatment of olefin oligomers via a boron trifluoride pr will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1816140

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.