ABSTRACT:
A thermal interface material (10) includes 100 parts by weight of a silicone oil (11) and 800˜1200 parts by weight of a metal powder (12) mixed into the silicone oil. An outer surface of each metal particle (121) of the metal powder is coated with a metal oxide layer (122). A method of producing the thermal interface material includes steps of: (1) applying a layer of organo coupling agent on the metal powder; (2) heating the metal powder at a temperature between 200 to 300° C. to coat a metal oxide layer on an outer surface of the metal powder; and (3) adding the metal powder with the coated metal oxide layer to a silicone oil. The thermal interface material has an excellent thermal conductivity and an excellent electrical insulating property.
REFERENCES:
patent: 3658311 (1972-04-01), Di Giambattista et al.
patent: 5213704 (1993-05-01), Anderson et al.
patent: 6040362 (2000-03-01), Mine et al.
patent: 6605238 (2003-08-01), Nguyen et al.
Cheng Ching-Tai
Cheng Nien-Tien
Foxconn Technology Co., Ltd.
Knapp Jeffrey T.
Moore Margaret G
LandOfFree
Thermal interface material and method of producing the same does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Thermal interface material and method of producing the same, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Thermal interface material and method of producing the same will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-4238892