ABSTRACT:
A coated article includes a superalloy substrate, an intermediate bond coat and a thermal barrier coating. The bond coat may include a platinum aluminide layer underlying a thin oxide layer. The thin oxide layer may include alumina. The coated article has high strength and durability at high temperatures over extended periods of time and thus is especially useful in the form of, e.g., a turbine blade or turbine vane.
REFERENCES:
patent: 3677789 (1972-07-01), Bungardt et al.
patent: 3692554 (1972-09-01), Bungardt et al.
patent: 3819338 (1974-06-01), Bungardt et al.
patent: 3961910 (1976-06-01), Baladjanian et al.
patent: 3979273 (1976-09-01), Panzera et al.
patent: 3999956 (1976-12-01), Stueber et al.
patent: 4123594 (1978-10-01), Chang
patent: 4123595 (1978-10-01), Chang
patent: 4137370 (1979-01-01), Fujishiro et al.
patent: 4321310 (1982-03-01), Ulion et al.
patent: 4321311 (1982-03-01), Strangman
patent: 4399199 (1983-08-01), McGill et al.
patent: 4401697 (1983-08-01), Strangman
patent: 4405659 (1983-09-01), Strangman
patent: 4405660 (1983-09-01), Ulion et al.
patent: 4414249 (1983-11-01), Ulion et al.
patent: 4477538 (1984-10-01), Clarke
patent: 4530885 (1985-07-01), Restall
patent: 4643951 (1987-02-01), Keem et al.
patent: 4676994 (1987-06-01), Demaray
patent: 4722869 (1988-02-01), Honda et al.
patent: 4880614 (1989-11-01), Strangman et al.
patent: 4916022 (1990-04-01), Solfest et al.
patent: 5015502 (1991-05-01), Strangman et al.
patent: 5180285 (1993-01-01), Lau
patent: 5236745 (1993-08-01), Gupta et al.
patent: 5238752 (1993-08-01), Duderstadt et al.
patent: 5350599 (1994-09-01), Rigney et al.
patent: 5427866 (1995-06-01), Nagaraj et al.
patent: 5500252 (1996-03-01), Meelu
patent: 5512382 (1996-04-01), Strangman
patent: 5514482 (1996-05-01), Strangman
patent: 5562998 (1996-10-01), Strangman
R. Lowrie, "Composite Coatings of CoCrAlY Plus Platinum", Thin Solid Films, 45 (1977), pp. 491-498.
Birks et al., "Introduction to High Temperature Oxidation of Metals", 1983, p. 128.
J. T. Prater et al., "Ceramic Thermal Barrier Coatings with Improved Corrosion Resistance", Surface and Coatings Technology, vol. 32, 1987, pp. 389-397.
A. McMinn et al., "Field Evaluation of Gas Turbine Protective Coatings", Journal of Engineering for Gas Turbines and Power, vol. 110, Jan. 1988, p. 142.
T. E. Stangman, "Thermal Barrier Coatings for Turbine Airfoils", Thin Solid Films, 127 (1985), pp. 93-105.
Bell Stanley R.
Rickerby David S.
White Daniel K.
Chromalloy United Kingdom Ltd.
King Roy V.
Rolls-Royce plc
LandOfFree
Thermal barrier coating for a superalloy article does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Thermal barrier coating for a superalloy article, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Thermal barrier coating for a superalloy article will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2197145