ABSTRACT:
A low alloy rotor steel is described which is substantially free of temper embrittlement within given constraints. In addition to describing the chemical composition there is included equations for predetermining the fracture appearance transition temperature of the unembrittled steel which equation permits the manufacturer to balance the alloying components within the ranges given in order to obtain a predetermined fracture appearance transition temperature, and by further balancing of the alloying components, the change in the fracture appearance transition temperature can be controlled to within .+-. 40F.degree.. Drawings are included which graphically depict the area for control of the critical relationship between the molybdenum and the chromium.
REFERENCES:
patent: 2968549 (1961-01-01), Brady et al.
patent: 3092491 (1963-06-01), Payson et al.
patent: 3201232 (1965-08-01), Thier
patent: 3291655 (1966-12-01), Gill et al.
Randig R. T.
Stallard W.
Westinghouse Electric Corporation
LandOfFree
Temper embrittlement free low alloy steel does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Temper embrittlement free low alloy steel, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Temper embrittlement free low alloy steel will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-675435