ABSTRACT:
A tear/puncture resistant semi-laminate material comprising a layer of woven polyethylene bonded to a layer of nonwoven polyethylene film impregnated with a volatile corrosion inhibitor. The layers are not bonded with a uniform layer of adhesive, but are semi-laminated by bonding at points or in strips at the edges of the respective layers or at discrete, discontinuous intervals across the width of the material. In an alternative embodiment, polypropylene is substituted for polyethylene.

REFERENCES:
patent: 2742388 (1956-04-01), Russell
patent: 3130647 (1964-04-01), Anderson et al.
patent: 3715251 (1973-02-01), Prentice
patent: 4668566 (1987-05-01), Braun
patent: 4748070 (1988-05-01), Beehler
patent: 4749423 (1988-06-01), Vaalberg et al.
patent: 5272023 (1993-12-01), Yamamoto et al.
patent: 5342469 (1994-08-01), Bodford et al.
patent: 5424115 (1995-06-01), Stokes

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Tear/puncture resistant semi-laminate material does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Tear/puncture resistant semi-laminate material, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Tear/puncture resistant semi-laminate material will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-702728

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.