Tannin treatment of aluminum

Metal treatment – Compositions – Heat treating

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

106 14, C23F 700

Patent

active

040544664

ABSTRACT:
Disclosed are a composition and process useful for the treatment of an aluminum surface comprising contacting the surface with an aqueous solution containing at least 0.000025 weight percent of a vegetable tannin, which solution exhibits a pH of at least 3. Best results can be obtained via a two-stage tanin treatment in which the treating solution of the first stage also contains titanium and fluoride in dissolved form.

REFERENCES:
patent: 2146840 (1939-02-01), Newsome et al.
patent: 2502441 (1950-04-01), Dodd et al.
patent: 2854368 (1958-09-01), Shreir
patent: 3443992 (1969-05-01), Schmidt et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Tannin treatment of aluminum does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Tannin treatment of aluminum, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Tannin treatment of aluminum will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1445458

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.