Chemical apparatus and process disinfecting – deodorizing – preser – Process disinfecting – preserving – deodorizing – or sterilizing – Maintaining environment nondestructive to metal
Reexamination Certificate
2006-12-19
2006-12-19
Bell, Bruce F. (Department: 1746)
Chemical apparatus and process disinfecting, deodorizing, preser
Process disinfecting, preserving, deodorizing, or sterilizing
Maintaining environment nondestructive to metal
C422S006000, C252S400540, C106S014050, C106S014210
Reexamination Certificate
active
07150852
ABSTRACT:
A method and system for preventing galvanic corrosion associated with a fastener of a first metal type and within an orifice of a second metal type for receiving said fastener. The method includes coating the fastener with a corrosive inhibitor and by further coating at least one of the fastener and orifice with an anaerobic composition that expands after the fastener is inserted into the orifice. The system includes a corrosive inhibitor coating at least a portion of the fastener adapted to contact the second metal type; and an anaerobic composition interposed between the corrosive inhibited portion of the fastener and orifice, and adapted to expand after the corrosive inhibitor portion of the fastener is inserted into the orifice.
REFERENCES:
patent: 4692988 (1987-09-01), Shulver et al.
patent: 5302679 (1994-04-01), Maandi et al.
patent: 5373075 (1994-12-01), Maandi
patent: 2002/0195592 (2002-12-01), Geer et al.
Beierle, legal representative Barbara
Senske Jules F.
Beam Robert Charles
Bell Bruce F.
Moran John F.
The United States of America as represented by the Secretary of
LandOfFree
System and method for reducing galvanic corrosion associated... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with System and method for reducing galvanic corrosion associated..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and System and method for reducing galvanic corrosion associated... will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-3671321