ABSTRACT:
A method and apparatus achieves making a surface-analysis determination precedent to allowing an electrofusion welding operation on pipe stock which is prescribed to be scraped, skinned or cleaned of surface contaminants prior to being graded ‘passable’ for such electrofusion welding. The method and apparatus utilizes non-contacting probes affixed to the welding power-supply leads such that inspection is automatic on the applicable pipe section(s) contemporaneously prior to enabling power-supply to the hot-wire welding coils. If the applicable pipe section fails the inspection, the welding equipment is disabled until the probes are disassembled, and then re-assembled for a succeeding inspection, such that during the interim an operator presumptively rectifies the situation as by re-scraping or skinning the applicable pipe section.
REFERENCES:
patent: 3973441 (1976-08-01), Porter
patent: 4213331 (1980-07-01), Porter
patent: 4435829 (1984-03-01), Siler et al.
patent: 4639580 (1987-01-01), Johnson
patent: 4663794 (1987-05-01), Evans
patent: 5116082 (1992-05-01), Handa et al.
patent: 5311785 (1994-05-01), Bar-Shay
patent: 5369248 (1994-11-01), Dufour et al.
patent: 5800247 (1998-09-01), Harms
patent: 5824179 (1998-10-01), Greig
patent: 5911895 (1999-06-01), Porfido et al.
patent: 6062948 (2000-05-01), Schiff et al.
patent: 6776874 (2004-08-01), Kobayashi et al.
patent: 6899785 (2005-05-01), Dutra et al.
patent: 07128305 (1995-05-01), None
Product Specification of electrofusion fittings of INNOGAZ® (of Monaco). product Nos. PE 2406 through PE 3408. dated Jan. 1999 (2 sheets).
Operating Manual for the Phoenix™ Electrofusion Processor of EF Technologies, Inc. (Of Newark, Delaware), published earlier than Aug. 2, 2002 (entire manual, comprising pp. 1-40 & front & back covers).
Product data for Lasercheck® gauge of the Optical Dimensions Co. (of Lake Forest, California), dated May 23, 2000 (6 sheets), from www.opticaldimensions.com.
Bay Jonathan A.
Hoang Tu
LandOfFree
Surface analysis preceding electrofusion of thermoplastics does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Surface analysis preceding electrofusion of thermoplastics, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Surface analysis preceding electrofusion of thermoplastics will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-3671476