Surface analysis preceding electrofusion of thermoplastics

Electric heating – Heating devices – With heater-unit housing – casing – or support means

Reexamination Certificate

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C219S221000, C219S230000, C219S544000

Reexamination Certificate

active

06858822

ABSTRACT:
A method and apparatus achieves making a surface-analysis determination precedent to allowing an electrofusion welding operation on pipe stock which is prescribed to be scraped, skinned or cleaned of surface contaminants prior to being graded ‘passable’ for such electrofusion welding. The method and apparatus utilizes non-contacting probes affixed to the welding power-supply leads such that inspection is automatic on the applicable pipe section(s) contemporaneously prior to enabling power-supply to the hot-wire welding coils. If the applicable pipe section fails the inspection, the welding equipment is disabled until the probes are disassembled, and then re-assembled for a succeeding inspection, such that during the interim an operator presumptively rectifies the situation as by re-scraping or skinning the applicable pipe section.

REFERENCES:
patent: 3973441 (1976-08-01), Porter
patent: 4213331 (1980-07-01), Porter
patent: 4435829 (1984-03-01), Siler et al.
patent: 4639580 (1987-01-01), Johnson
patent: 4663794 (1987-05-01), Evans
patent: 5116082 (1992-05-01), Handa et al.
patent: 5311785 (1994-05-01), Bar-Shay
patent: 5369248 (1994-11-01), Dufour et al.
patent: 5800247 (1998-09-01), Harms
patent: 5824179 (1998-10-01), Greig
patent: 5911895 (1999-06-01), Porfido et al.
patent: 6062948 (2000-05-01), Schiff et al.
patent: 07128305 (1995-05-01), None
Product Specification of electrofusion fittings of INNOGAZ® (of Monaco), product Nos. PE 2406 through PE 3408, dated 01-99 (2 sheets).
Operating Manual for the Phoenix™ Electrofusion Processor of EF Technologies, Inc. (Of Newark, Delaware). published earlier than Aug. 2, 2002 (entire manual, comprising pp. 1-40 & front & back covers).
Product data for Lasercheck® gauge of the Optical Dimensions Co. (of Lake Forest, California), dated May 23, 2000 (6 sheets), from www.opticaldimensions.com.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Surface analysis preceding electrofusion of thermoplastics does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Surface analysis preceding electrofusion of thermoplastics, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Surface analysis preceding electrofusion of thermoplastics will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3476661

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.