ABSTRACT:
Superalloys containing uniform dispersions of at least 0.1 volume percent of a metal nitride improve qualities of superalloys. These superalloys are produced from superalloy powders by a nitridng process utilizing a controlled atmosphere for controlled times at controlled temperature. A nitriding temperature of at least 700.degree. C is required in order to produce effective amounts of nitride in practical lengths of time.
REFERENCES:
patent: 2823988 (1958-02-01), Grant et al.
patent: 3459546 (1969-08-01), Lambert
patent: 3720551 (1973-03-01), Allen
Lin Ching San
Smith James Thomas
Castle Donald R.
GTE Sylvania Incorporated
Hunt Brooks H.
McNeill William H.
O'Malley Norman J.
LandOfFree
Superalloys containing nitrides and process for producing same does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Superalloys containing nitrides and process for producing same, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Superalloys containing nitrides and process for producing same will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1476772