Specialized metallurgical processes – compositions for use therei – Compositions – Consolidated metal powder compositions
Patent
1987-08-28
1989-01-17
Terapane, John F.
Specialized metallurgical processes, compositions for use therei
Compositions
Consolidated metal powder compositions
75233, C22C 2912
Patent
active
047986255
ABSTRACT:
Superalloy with oxide dispersion hardening having improved corrosion and oxidation resistance and based on nickel with the following composition:
REFERENCES:
patent: 3660049 (1972-05-01), Benjamin
patent: 3728088 (1973-04-01), Benjamin
patent: 3738817 (1973-06-01), Benjamin
patent: 3743548 (1973-07-01), Baranow et al.
patent: 3749612 (1973-07-01), Benjamin et al.
patent: 3776704 (1973-12-01), Benjamin
patent: 3809545 (1974-05-01), Benjamin
patent: 3920489 (1975-11-01), Buchanan
patent: 4080204 (1978-03-01), Ponzera
patent: 4599214 (1986-07-01), Luton
patent: 4631082 (1986-12-01), Andrews et al.
Jongenburger Peter
Singer Robert
BBC Brown Boveri AG
Jorgensen Eric
Terapane John F.
LandOfFree
Superalloy with oxide dispersion hardening having improved corro does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Superalloy with oxide dispersion hardening having improved corro, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Superalloy with oxide dispersion hardening having improved corro will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2412727