ABSTRACT:
A process for producing a fine grain forged superalloy article having a high yield strength at intermediate temperatures. A preferred starting composition comprises, by weight, 15% Cr, 13.6% Co, 4.1% Mo, 4.6% Ti, 2.2% Al, 0.01% C, 0.007% B, 0.07% Zr, balance Ni. This material is forged at a temperature above the gamma prime solvus and at a true strain of at least 0.5. Alternately, the material may be forged below the gamma prime solvus temperature with intermediate super solvus anneals. The overaged material is then worked at a temperature below the gamma prime solvus. The resultant fine grain material is then heat treated or can be further isothermally forged prior to heat treatment to produce complex shapes.
REFERENCES:
patent: 2977222 (1961-03-01), Bieber
patent: 3519503 (1970-07-01), Moore et al.
patent: 3677830 (1972-07-01), Cox et al.
patent: 3871223 (1975-03-01), Kralowetz et al.
patent: 3889514 (1975-06-01), Kralowetz et al.
patent: 4083734 (1978-04-01), Boesch
patent: 4430881 (1984-02-01), Kralowetz
patent: 4453985 (1984-06-01), Gessinger et al.
patent: 4574015 (1986-03-01), Genereux et al.
patent: 4579602 (1986-04-01), Paulonis et al.
patent: 4685977 (1987-08-01), Chang
patent: 4769087 (1988-09-01), Genereux et al.
patent: 4820353 (1989-04-01), Chang
patent: 4957567 (1990-09-01), Kuueger
patent: 5120373 (1992-06-01), Miller et al.
Athey Roy L.
Fuesting Timothy P.
Genereux Paul D.
Gostic William J.
Miller John A.
Phipps Margery S.
Simmons David A.
Sohl Charles E.
United Technologies Corporation
LandOfFree
Superalloy forging process does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Superalloy forging process, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Superalloy forging process will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-798005