ABSTRACT:
Superalloy with a nickel base matrix having good mechanical properties when ot in respect of tensile strength, creep resistance, low cycle fatigue and resistance to crack-propagation of which the composition in percentages by weight is as follows: Cr 11 to 13; Co 8 to 17; Mo 6 to 8; Nb less than or equal to 1.5; Ti 4 to 5; Al 4 to 5; Hf less than or equal to 1; C, B, Zr each less than or equal to 500 ppm; Ni remainder to 100. The alloy can be manufactured advantageously by powder metallurgy techniques and used in the manufacture of turbo machine disks.
REFERENCES:
patent: 3494709 (1970-02-01), Piearcey
Davidson James H.
Ducrocq Christian A. B.
Lestrat Didier P. A.
Marty Michel
Paintendre Bernard
Association pour la Recherche et le Developpement des Methodes e
Dean R.
Office National d'Etudes et de Recherches Aerospatiales - "O.N.E
Phipps Margery S.
Societe Nationale d'Etude et de Construction de Moteurs d'Aviati
LandOfFree
Superalloy compositions with a nickel base does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Superalloy compositions with a nickel base, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Superalloy compositions with a nickel base will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2347418