ABSTRACT:
The addition of small amounts of rhenium, technitium and their mixtures and, optionally erbium, to a nickel based superalloy consisting essentially of 19.3-19.7 weight percent chromium, about 0.5% carbon, about 2.5% iron, the balance essentially nickel, provides enhanced mechanical properties particularly suitable for applications in gas turbine engine components.

REFERENCES:
patent: 3124452 (1964-03-01), Kraft
patent: 3554817 (1971-01-01), Thompson
patent: 3564940 (1971-02-01), Thompson et al.
patent: 3671223 (1972-06-01), Thompson et al.
patent: 3793010 (1974-02-01), Lempkey et al.
patent: 4012241 (1977-03-01), Lempkey et al.
patent: 4111723 (1978-09-01), Lempkey
patent: 4543235 (1985-09-01), Lempkey et al.
"The Influence of Off-Axis Reinforcement of the Tensile Strength of an Ni-Al-Cr-C Eutectic Composite", by G. J. May, Journal of Materials Science, 10(1975), 77-82.
"The Fatigue Behavior of an Aligned Ni-Al-Cr-C Eutectic Alloy", G. J. May, Metallurgical Transactions, vol. 6A, May 1975.
"Creep Behavior of a Ni-Ni.sub.3 Al--Cr.sub.3 C.sub.2 Eutectic Composite", Bullock et al., Acta Metallurgica, vol. 25, pp. 333--334, 1977.
"The Contribution of Fibre Reinforcement to the Tensile and Creep Strengths of --.sup.1 -Cr.sub.3 C.sub.2 Eutectic Composite", Miles et al., published in the Proceedings of the Second Conference on In Situ Composites, 1976.
"Effects of Alloying Additions and High Rate Solidification on the Mechanical and Oxidation Behavior of the Directionally Solidified--.sup.1 -Cr.sub.3 C.sub.2 Eutectic", Bullock et al.
"Exeltrodeposition of Rhenium-Nickel Alloys from Ammoniacal Citrate Solution", Fukushima et al. Kunzoku Hyomem Gijutsu 36, 198-203, 1985.
"Effect of Rhenium on the Physical Properties of Iron-Nickel Alloys", Doroshek et al. Issled. Premen. Splavov Tugoplavkikh Met., 147-150, 1983.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Superalloy compositions and articles does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Superalloy compositions and articles, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Superalloy compositions and articles will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2416706

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.