ABSTRACT:
A coated superalloy component includes a substrate article formed of a superalloy and an adherent coating over the substrate. The coating is a nickel-base superalloy containing 0.3 volume percent or more of a dispersed oxide of yttrium, hafnium and/or a rare earth, and, preferably, grain boundary strengthening elements such as carbon, zirconium, and boron. The oxide dispersoids improve the performance of the coating in service, reducing the incidence failures due to thermal fatigue, oxidation, and corrosion damage. The dispersoid-containing coating may be formed by directly depositing the oxide-containing coating, or by depositing a metallic coating under conditions which permit the formation of such dispersoids during the deposition process.
REFERENCES:
patent: 3776704 (1973-12-01), Benjamin
patent: 3864093 (1975-02-01), Woljla
patent: 4029477 (1977-06-01), Grisik
patent: 4101713 (1978-07-01), Hirsch et al.
patent: 4111685 (1978-09-01), Baranow
patent: 4169742 (1979-10-01), Wukusick et al.
patent: 4198442 (1980-04-01), Gupta et al.
patent: 4230748 (1980-10-01), Patel
patent: 4237193 (1980-12-01), Jackson et al.
patent: 4275090 (1981-06-01), McComas
patent: 4313760 (1982-02-01), Dardi et al.
patent: 4339509 (1982-07-01), Dardi et al.
patent: 4404263 (1983-09-01), Hodes et al.
patent: 4446199 (1984-05-01), Gedwill et al.
patent: 4569824 (1986-02-01), Duhl et al.
patent: 4717435 (1988-01-01), Kawasaki et al.
patent: 4758480 (1988-07-01), Hecht et al.
patent: 4764225 (1988-08-01), Shankar et al.
patent: 4921405 (1990-05-01), Wilson
patent: 4961818 (1990-10-01), Benn
patent: 4995922 (1991-02-01), Jongenburger
patent: 5043138 (1991-08-01), Darolia et al.
patent: 5141821 (1992-08-01), Lugscheider et al.
patent: 5240491 (1993-08-01), Budinger et al.
Metals Handbook, Tenth Edition TA 459 M43, 1990, pp. 950-957.
"Databook", 1978, Metal Progress Mid-Jun. 1978, p. 106, (No Month).
"East, Handbook of Chemistry and Physics", 57th Ed, CRC Press Inc, QD 65 C4 1976-1977, pp. 116, 135, 175 (No Month).
Thin Solid Films, vol. 173, No. 1, Jun. 1, 1989, Lausanne, CH, pp. 99-107; B. Gudmundsson `Yttrium Oxides in Vacuum-Plasma-Sprayed CoNiCrALY Coatings` p. 100, paragraph 2.3.
WO-A-8 706 273, Publication Date Oct. 22, 1987. Title: Coating to Protect Against Wear and Fretting Corrosion of, in Particular, Metal Mechanical Components Held Together by Frictional Adherence.
Darolia Ramgopal
Goldman Edward Harvey
Wortman David John
General Electric Company
Hess Andrew C.
Narciso David L.
Nguyen Ngoc-Yen
LandOfFree
Superalloy component with dispersion-containing protective coati does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Superalloy component with dispersion-containing protective coati, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Superalloy component with dispersion-containing protective coati will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-340389